Process - How it works

 

If you have not seen it before, theT-DRILL process works like this...

1. The T-DRILL Power legs center on the main pipe. Pilot hole is drilled.

2. On the Inside of the main pipe, from the T-DRILLhead special hardened steel formation pins are extended. These cause a back flow of rigid metal at the root radius of the joint. The result is a 5.5% average thickening at the root radius.
3. As the T-DRILLhead is extracted by power feed, the formation pins extrude an outlet around the pilot hole. Power legs absorb all rotational torque.
p1 p2 p3
p4 p5 p6
4. Tube End Notcher cuts a coupon and double dimples branch tube to assure free flow and limit depth of insertion into main line providing an inspection aid.
5. The branch tube is inserted into the outlet and brazed to provide a solid, free-flow joint. Double dimples are in line with the flow of the tube.
6. The branch outlets are as strong as the tube. One lead-free brazed joint replaces three soldered joints needed for a tee fitting.
     
 
 